Diseño · Acero

Límite de corte a fatiga Δσ,L (EN 1993-1-9)

  • Tipo: Propiedad
  • Versión 1
  • revisado el 24/11/2026

Límite de corte para rangos de tensión normal a 100 millones de ciclos según EN 1993-1-9 cláusula 7.1(1): ΔσL = 0,549 · ΔσD.

ΔσL=0.549⋅ΔσD\displaystyle \Delta\sigma_{L} = 0.549 \cdot \Delta\sigma_{D}
  • EN 1993-1-9:2005
Apply in CALC

Catalog formula, not a design. Check input values, coefficients, and limits against the standard and its national annex.

ΔσDΔσL

Formula and quantities

SymbolNameUnitNote
ΔσD\displaystyle \Delta\sigma_{D}Límite de fatiga de amplitud constanteN/m²
ΔσL\displaystyle \Delta\sigma_{L}Límite de corte a fatigaN/m²Result

Ejemplo resuelto

ΔσD\displaystyle \Delta\sigma_{D} = 58.960.000 N/m²

ΔσL\displaystyle \Delta\sigma_{L} = 32.369.000 N/m²

Standard and source

Standard
EN 1993-1-9:2005
Result
ΔσL\displaystyle \Delta\sigma_{L} in MPa

Reference to clause and equation, no standard text. The description is written in our own words.

Try it

Unit system
ΔσL\displaystyle \Delta\sigma_{L} = 32.369.000 N/m²= 0.549 · (58.960.000 N/m²)

Continue with Mia

Fills the input field in CALC; nothing is sent until you send it.

No matching formula yet? Find the right calculation rule.

Describe what you want to determine. Mia searches the formula catalog first and clarifies assumptions before anything is calculated.

La búsqueda comienza en Diseño › Acero.

Miaknows the formula catalog and asks for what is missing.

You clarify missing information with Mia in the next step. Nothing is calculated yet.