설계 · 알루미늄
HAZ 감소 0.2 % 내력 fo,haz
용접부 인접 열영향부(HAZ)에서 감소된 0.2 % 내력: fo,haz = ρo,haz · fo.
Catalog formula, not a design. Check input values, coefficients, and limits against the standard and its national annex.
Formula and quantities
| Symbol | Name | Unit | Note |
|---|---|---|---|
| 0.2 % 내력에 대한 HAZ 연화 계수 | 1 | ||
| 모재의 특성 0.2 % 내력 | N/m² | ||
| HAZ 감소 0.2 % 내력 | N/m² | Result |
예제
= 0.5 · = 260,000,000 N/m²
= 130,000,000 N/m²
Standard and source
- Standard
- EN 1999-1-1:2007
- Result
- in MPa