设计 · 混凝土

500°C 等温线法折减有效高度 (EN 1992-1-2)

  • 类型:属性
  • 版本1
  • 2026/11/21已审核

根据 EN 1992-1-2 附录 B.1 受压面或受拉面受火混凝土梁或板的折减有效高度 dfi:dfi = d - a500。

dfi=d−a500\displaystyle d_{fi} = d - a_{500}
Apply in CALC

Catalog formula, not a design. Check input values, coefficients, and limits against the standard and its national annex.

dfi

Formula and quantities

SymbolNameUnitNote
d\displaystyle d原始有效高度mm
a500\displaystyle a_{500}受火受压面至 500°C 等温线的深度mm
dfi\displaystyle d_{fi}火灾下折减有效高度mmResult

实例

d\displaystyle d = 550 mm · a500\displaystyle a_{500} = 35 mm

dfi\displaystyle d_{fi} = 515 mm

Standard and source

Result
dfi\displaystyle d_{fi} in mm

Reference to clause and equation, no standard text. The description is written in our own words.

Try it

Unit system
dfi\displaystyle d_{fi} = 515 mm= (550 mm) - (35 mm)

Continue with Mia

Fills the input field in CALC; nothing is sent until you send it.

No matching formula yet? Find the right calculation rule.

Describe what you want to determine. Mia searches the formula catalog first and clarifies assumptions before anything is calculated.

检索将在 设计 › 混凝土 开始。

Miaknows the formula catalog and asks for what is missing.

You clarify missing information with Mia in the next step. Nothing is calculated yet.